OverviewThis collection explores all aspects of metallurgical processing, materials behavior, and microstructural performance for the distinct class of 718-type superalloys and derivatives. Technical topics focus on alloy and process development, production, product applications, trends, and the development of advanced modeling tools. New developments in R&D, new processing methods, 3D printing, and other nontraditional applications also are covered. Full Product DetailsAuthor: Eric A. Ott , Joel Andersson , Chantal Sudbrack , Zhongnan BiPublisher: Springer International Publishing AG Imprint: Springer International Publishing AG Edition: 1st ed. 2023 Weight: 1.616kg ISBN: 9783031274466ISBN 10: 3031274466 Pages: 836 Publication Date: 21 April 2023 Audience: Professional and scholarly , Professional & Vocational Format: Hardback Publisher's Status: Active Availability: Manufactured on demand ![]() We will order this item for you from a manufactured on demand supplier. Table of ContentsReviewsAuthor InformationEric A. Ott, GE Aviation, West Chester, OH, USA; Joel Andersson, University West, Trollhättan, Sweden; Chantal Sudbrack, U.S. DOE National Energy Technology Laboratory, Albany, OR, USA; Zhongnan Bi, Central Iron and Steel Research Institute, Beijing, China; Kevin Bockenstedt, ATI Specialty Materials, Monroe, NC, USA; Ian Dempster, Wyman Gordon / PPC, Houston, TX, USA; Michael Fahrmann, Haynes International, Kokomo, IN, USA; Paul Jablonski, U.S. DOE National Energy Technology Laboratory, Albany, OR, USA; Michael Kirka, Oak Ridge National Laboratory, Oak Ridge, TN, USA; Xingbo Liu, West Virginia University, Morgantown, WV, USA; Daisuke Nagahama, Honda R&D Co Ltd, Wako-shi, Saitama, Japan; Tim Smith, NASA Glenn Research Center, Cleveland, OH, USA; Martin Stockinger, Montanuniversität Leoben, Kapfenberg, Styria, Austria; Andrew Wessman, The University of Arizona, Tucson, AZ, USA Tab Content 6Author Website:Countries AvailableAll regions |