OverviewStress corrosion cracking is a major problem in light water nuclear reactors, whether pressurised water reactors (PWRs) or boiling water reactors (BWRs). The nuclear industry needs to be able to predict the service life of these power plants and develop appropriate maintenance and repair practices to ensure safe long term operation. This important book sums up key recent research on corrosion in light water reactors and its practical applications. The book is divided into four parts. It begins with an overview of materials degradation due to stress corrosion, corrosion potential monitoring and passivation. Part two summarises research on susceptibility of materials to stress corrosion cracking and the ways it can be initiated. The third part of the book considers stress corrosion crack propagation processes whilst the final part includes practical case studies of corrosion in particular plants. The book reviews corrosion in a range of materials such as low alloy steels, stainless steels and nickel-based alloys. With its distinguished editor and team of contributors, Corrosion issues in light water reactors is a standard work for the nuclear industry. Summarises key recent research on corrosion in light water reactorsIncludes practical case studies Full Product DetailsAuthor: J-M OlivePublisher: Woodhead Publishing Imprint: Woodhead Publishing ISBN: 9781306381703ISBN 10: 1306381703 Pages: 369 Publication Date: 01 January 2007 Audience: General/trade , General Format: Electronic book text Publisher's Status: Active Availability: Available To Order ![]() We have confirmation that this item is in stock with the supplier. It will be ordered in for you and dispatched immediately. Table of ContentsReviewsAuthor InformationTab Content 6Author Website:Countries AvailableAll regions |